Robalon® FG PE PE-UHMW PE 1000
Get Latest PriceGreiðsla Tegund: | T/T,Paypal |
Incoterm: | FOB,CFR,CIF,EXW,DDP,DDU |
Mín. Order: | 1 Kilogram |
Samgöngur: | Ocean,Land,Air,Express |
Höfn: | Shenzhen,Guangzhou,Hongkong |
Greiðsla Tegund: | T/T,Paypal |
Incoterm: | FOB,CFR,CIF,EXW,DDP,DDU |
Mín. Order: | 1 Kilogram |
Samgöngur: | Ocean,Land,Air,Express |
Höfn: | Shenzhen,Guangzhou,Hongkong |
Gerð nr.: Robalon® FG PE
Merki: Robalon
Selja einingar | : | Kilogram |
Pakkagerð | : | Útflutningspakki |
The file is encrypted. Please fill in the following information to continue accessing it
Robalon® FG PE - PE -UHMW - PE 1000
Litur hvítur. Engin molybden disulfide ál, engin krossbinding. Lífeðlisfræðilega öruggt. Plast okkar er í samræmi við kröfur ESB-reglugerðarinnar 10/11/ESB, sem gildir síðan í maí 2011, breyting þess 1282/2011/ESB auk ramma reglugerðar 1935/2004/EB og reglugerðin 2023/2006/EB . Auðvitað eru framleiðsluferlar okkar háð heimspekinni „góð framleiðsluvenja“ (2023/2006/EG).
Einkenni
Lífeðlisfræðilega öruggt
Góð renni- og slithegðun
Matvælasamhæfi samkvæmt 10/11/ESB, 1935/2004/EB, FDA
Atvinnugreinar
Drykkja og úrgangsvatnstækni
Vélaverkfræðiiðnaður
Matvælaiðnaður
Landbúnaðariðnaður
Alpageirinn
Tæknilegar upplýsingar Robalon® FG
General properties | |||
Test Method | Unit | Guideline Value | |
Density | DIN EN ISO 1183-1 | g / cm3 | 0,93 |
Water absorption | DIN EN ISO 62 | % | <0,01 |
Flammability (Thickness 3 mm / 6 mm) | UL 94 | HB/HB | |
Molecular weight | g/mol | 9,20 * 106 | |
Color | white | ||
Mechanical properties | |||
Test Method | Unit | Guideline Value | |
Yield stress | DIN EN ISO 527 | MPa | 17 |
Elongation at break | DIN EN ISO 527 | % | >300 |
Tensile modulus of elasticity | DIN EN ISO 527 | MPa | 470 |
Notched impact strength | DIN EN ISO 179/1eA | kJ / m2 | >100 |
Shore hardness | DIN EN ISO 868 / 15 sec | scale D | 63 |
Compression - compression set | 23°C, 2N/mm², 1h | % | ∼2 |
Compression - compression set | 80°C, 10N/mm², 56h | % | ∼20 |
Thermal properties | |||
Test Method | Unit | Guideline Value | |
Melting temperature | DIN EN ISO 3146 | 掳C | 135 |
Thermal conductivity | DIN EN ISO 8302 | W / (m * K) | 0,41 |
Thermal capacity | DIN 51005 | kJ / (kg * K) | 1,84 |
Coefficient of linear thermal expansion | DIN 53752 | 10-6/ K | 200 |
Service temperature, long term | Average | ℃ | -200 ... 80 |
Service temperature, short term (max.) | Average | ℃ | 110 |
Electrical properties | |||
Test Method | Unit | Guideline Value | |
Dielectric constant | IEC 60250 | 2,1 ... 3 | |
Dielectric dissipation factor (106聽Hz) | IEC 60250 | 10 * 10-4 | |
Dielectric dissipation factor (100 Hz) | IEC 60250 | 3,9 * 10-4 | |
Volume resistivity | DIN EN 62631-3-1 | Ohm * cm | 1012 |
Surface resistivity | DIN EN 62631-3-2 | Ohm | 1012 |
Comparative tracking index | IEC 60112 | 600 | |
Dielectric strength | IEC 60243 | kV / mm | 45 |
Persónuverndaryfirlýsing: Persónuvernd þín er mjög mikilvæg fyrir okkur. Fyrirtækið okkar lofar ekki að birta persónulegar upplýsingar þínar til allra útgjalda með skýrum heimildum þínum.
Fylltu út frekari upplýsingar svo það geti haft samband við þig hraðar
Persónuverndaryfirlýsing: Persónuvernd þín er mjög mikilvæg fyrir okkur. Fyrirtækið okkar lofar ekki að birta persónulegar upplýsingar þínar til allra útgjalda með skýrum heimildum þínum.